A first class brick should have a minimum crushing strength of
Show answer & solution
Answer: (B) 10.5 MN/m²
A first-class brick must possess a minimum compressive strength of 10.5 MN/m² (approx. 105 kg/cm²).
Civil Engineering · Building Materials
49 questions, each with the answer and a worked solution.
Practice interactively and track your score →A first class brick should have a minimum crushing strength of
Answer: (B) 10.5 MN/m²
A first-class brick must possess a minimum compressive strength of 10.5 MN/m² (approx. 105 kg/cm²).
A first class brick should not absorb water more than _____________ of its own dry weight after 24 hours immersion in cold water.
Answer: (C) 20%
First-class bricks are well-burnt and dense, absorbing no more than 20% of their dry weight in water after 24 hours.
A frog (a shallow depression) provided on one face of a brick during molding serves mainly to
Answer: (A) reduce the weight of the brick, and provide a key for better mortar bond in masonry construction
The frog lightens the brick slightly and, once filled with mortar, improves the mechanical key between courses.
A good quality building brick should generally give, when struck with another brick or a hammer, a
Answer: (B) clear, metallic ringing sound, indicating a well-burnt, sound brick
A sharp, ringing sound is the traditional field test for a well-burnt, sound brick.
A good quality building brick should generally have a minimum compressive strength of approximately (varying by class/grade specified)
Answer: (A) 3.5 N/mm2 or higher, for common structural classes (with higher-grade bricks having correspondingly higher strength)
Common structural brick grades specify a minimum compressive strength typically starting around 3.5 N/mm2.
A good quality building brick, when broken, should show a
Answer: (A) uniform, homogeneous, compact texture, free from visible flaws, cracks, or excessive lumps
A good brick's broken cross-section should be uniform, compact, and free of visible defects.
A high degree of efflorescence in bricks is generally considered a
Answer: (B) undesirable defect, since it indicates the presence of harmful soluble salts, which can also contribute to spalling or other deterioration of the masonry over time
Heavy efflorescence signals harmful soluble salt content that can also drive spalling and long-term deterioration.
As per common specification limits, the water absorption of a good quality first-class building brick, after 24 hours of soaking, should generally not exceed about
Answer: (B) 20% (with variations by specification/class)
First-class bricks are typically specified to have water absorption not exceeding roughly 20%, varying by standard.
Bricks are commonly classified by grade or class (such as first class, second class, third class) mainly based on their
Answer: (B) quality characteristics, such as compressive strength, water absorption, dimensional accuracy, and freedom from defects/cracks
Brick class/grade is based on measured quality parameters, not color, brand, or origin alone.
Efflorescence on the surface of brick masonry appears as a
Answer: (A) whitish, powdery or crystalline deposit, caused by soluble salts within the bricks (or mortar) migrating to the surface and crystallizing as moisture evaporates
Efflorescence is the characteristic white salt deposit left as moisture carrying soluble salts evaporates from the surface.
Fly ash bricks, an alternative to traditional clay bricks, are manufactured mainly using
Answer: (A) fly ash (a byproduct of coal-fired power generation) combined with materials such as lime, gypsum, and/or cement, without necessarily requiring the same high-temperature firing as clay bricks
Fly ash bricks combine the power-plant byproduct with binders like lime/gypsum/cement, often without high-temperature firing.
For one cubic metre of brick masonry, the number of bricks required are
Answer: (C) 500
Standard estimation rules account for mortar joints, requiring approximately 500 standard modular bricks per cubic meter of brick masonry.
Hand-molded (or ground-molded) bricks, as compared to machine-made (e.g., wire-cut) bricks, are generally
Answer: (B) somewhat less uniform in size, shape, and quality, being more dependent on the skill of the individual brick-maker
Hand molding depends more on individual craftsmanship, generally giving less consistency than mechanical methods.
Jhama bricks are
Answer: (D) over burnt with irregular shape
Jhama bricks are heavily over-burnt bricks that get distorted in shape and fused together, though sometimes used as road metal or foundation concrete aggregate.
One environmental advantage often cited for fly ash bricks, compared to traditional clay bricks, is that they
Answer: (B) can utilize a waste byproduct (fly ash) and, in many manufacturing processes, avoid the need for high-temperature kiln firing (and its associated fuel consumption/emissions), unlike traditional clay bricks
Fly ash bricks recycle waste and typically skip fuel-intensive firing, reducing both waste and emissions compared to clay bricks.
Over-burnt bricks, resulting from excessive firing temperature or duration, are generally characterized by
Answer: (B) being hard, sometimes brittle or distorted/vitrified, and can be over-hard for some purposes, though sound over-burnt bricks (not badly distorted) can still be usable, even good, for certain purposes
Overburning can distort/vitrify bricks, but sound, undistorted overburnt bricks can still be usable, sometimes valued for their hardness.
Perforated (or hollow) bricks, having holes/cavities through their body, are generally used mainly to
Answer: (B) reduce the weight of the brick and improve its thermal insulation properties, while often using less raw material per brick
Perforations lighten bricks, improve insulation, and reduce raw material use, while still providing adequate strength.
The average out-turn of first class bricks in clamp burning is about
Answer: (B) 60%
Clamps (povas) are traditional intermittent kilns yielding a lower percentage (around 60%) of first-class bricks compared to modern continuous kilns.
The average out-turn of first class bricks in kiln burning is
Answer: (C) 70 to 80%
Modern continuous kilns (such as Bull's trench kilns or Hoffman kilns) provide uniform heat control, yielding 70% to 80% first-class bricks.
The brick earth is derived by the disintegration of _____________ rocks.
Answer: (A) igneous
Brick clay is primarily formed through the weathering, disintegration, and decomposition of igneous rocks like granite.
The bricks after burning in kilns require about _____________ days to cool down for unloading.
Answer: (D) 12
Kiln-burnt bricks require roughly 12 days of gradual cooling before workers can safely unload them.
The bricks after moulding should be dried in
Answer: (C) air for 3 to 8 days but not in sun
Bricks must be dried slowly in shaded air for 3 to 8 days to prevent rapid moisture evaporation, which causes warping and cracking.
The bricks should be burnt at temperature from
Answer: (D) 1000°C to 1200°C
Full vitrification and burning of clay bricks occur in the temperature range of 1000°C to 1200°C.
The burning of bricks in kilns is complete within _____________ hours.
Answer: (C) 48
The active burning phase in standard continuous brick kilns takes approximately 48 hours.
The compressive strength of paving bricks should not be less than
Answer: (C) 40 MN/m²
Paving bricks are subjected to heavy abrasive traffic loads and require a high minimum compressive strength of 40 MN/m².
The compressive strength of perforated bricks should not be less than
Answer: (D) 7 MN/m²
Perforated clay bricks used in lightweight partition wall construction must maintain a minimum compressive strength of 7 MN/m².
The compressive strength of second class bricks should not be less than
Answer: (A) 7.5 MN/m²
Second-class bricks have slightly lower quality and burning standards, with a minimum required crushing strength of 7.5 MN/m².
The compressive strength test on bricks is used to determine the
Answer: (A) maximum load per unit area a brick can withstand before crushing, an important property for load-bearing masonry
Compressive strength testing directly measures a brick's crushing resistance, critical for load-bearing use.
The dolomite bricks are
Answer: (C) basic refractory bricks
Dolomite refractories contain magnesium and calcium oxides, classifying them as basic refractory bricks used in industrial metal-melting furnaces.
The frog of a brick is normally made on its
Answer: (D) top face
Frogs are traditionally placed on the top face of laid bricks so that mortar fills the depression from the layer above.
The good clay for making bricks is
Answer: (B) weathered clay
Weathered clay has been exposed to natural atmospheric elements, oxidizing impurities and improving homogeneity and plasticity.
The handmade bricks are _____________ to machine made bricks for facing purposes.
Answer: (A) superior
Handmade bricks often feature unique textures and aesthetic irregularities preferred for high-end architectural facing.
The indentation marks left on bricks during the process of moulding, are known as
Answer: (B) frogs
A frog is a depression molded onto the top face of a brick to form a key for mortar bonding.
The main raw material used for manufacturing ordinary clay bricks is
Answer: (A) suitable natural clay (brick earth), typically containing silica, alumina, lime, and iron oxide in appropriate proportions
Ordinary bricks are made from suitably composed natural clay (brick earth).
The manufacturing of clay bricks broadly involves the stages of
Answer: (A) preparation of clay, molding, drying, and burning (firing)
Standard brick-making follows clay preparation, molding, drying, then firing.
The natural drying of bricks is also called hack drying.
Answer: (A) True
Stacking unburnt bricks in rows (hacks) for natural atmospheric drying is termed hack drying.
The percentage of alumina in a good brick clay should vary from
Answer: (A) 20 to 30%
Good brick clay contains 20% to 30% alumina, giving it the necessary plasticity for molding.
The percentage of silica in a good brick clay should vary from
Answer: (D) 50 to 60%
Silica is the major component of brick earth, constituting 50% to 60%, preventing cracking and shrinking.
The principal constituent of every kind of brick earth is alumina.
Answer: (A) True
Alumina is the binding agent present in all brick clay, providing plasticity when mixed with water.
The process of mixing clay, water and other ingredients to make bricks, is known as
Answer: (B) pugging
Pugging is the thorough mechanical mixing and kneading of brick earth with water inside a pug mill to achieve uniform plasticity.
The size of a standard modular brick, as per one common specification, is approximately
Answer: (A) 190 mm x 90 mm x 90 mm (which, with 10 mm mortar joints, gives a nominal size of 200 mm x 100 mm x 100 mm)
A common modular brick actual size is 190x90x90 mm, becoming 200x100x100 mm nominal with a 10 mm mortar joint.
The size of mould for bricks should be _____________ the specified size of the bricks.
Answer: (C) larger than
Brick molds are manufactured slightly larger than the final required size to compensate for drying and burning shrinkage.
The standard size of a masonry brick is 20 cm × 10 cm × 10 cm.
Answer: (A) Agree
Standard modular brick dimensions with mortar joints measure 20 cm × 10 cm × 10 cm (or 19 cm × 9 cm × 9 cm nominal without mortar).
The water absorption test on bricks, typically conducted by soaking a brick in water for a specified period (such as 24 hours), is used to assess the brick's
Answer: (B) porosity, which relates to its durability and resistance to weathering
Water absorption reflects a brick's porosity, an indicator of its long-term durability and weathering resistance.
Under-burnt bricks, resulting from insufficient firing temperature or duration, are generally characterized by
Answer: (B) softer texture, lower strength, and a tendency to absorb more water, being generally of inferior quality
Insufficient firing leaves bricks soft, weak, and overly absorbent, marking them as poor quality.
Which of the following constituent, when present in excess quantity in clay causes the bricks to melt and distort during burning?
Answer: (C) Lime
Excess lime acts as a powerful flux, lowering the vitrification point and causing bricks to melt and distort during kiln burning.
Wire-cut bricks are manufactured by
Answer: (A) extruding a stiff, plastic clay through a die to form a continuous column, which is then cut into individual bricks using tensioned wires
Wire-cut bricks are extruded as a continuous clay column and then sliced into individual units by wires.
Excess of alumina in the clay
Answer: (B) makes the brick crack and warp on drying
Too much alumina causes excessive shrinkage, leading to heavy cracking and warping as the bricks dry.
Excess of silica in the clay
Answer: (A) makes the brick brittle and weak
An excess of free silica destroys the cohesion between clay particles, rendering the burnt bricks brittle and weak.