Process Equipment & Plant Design: Materials and Corrosion

Chemical Engineering · Process Equipment & Plant Design

43 questions, each with the answer and a worked solution.

Practice interactively and track your score →
Question 1

What is the most widely used material of construction in chemical plants for non-corrosive service?

  1. Titanium
  2. Carbon steel
  3. Platinum
  4. Glass
Show answer & solution

Answer: (B) Carbon steel

It is cheap, strong and easily fabricated.

Question 2

What makes stainless steel corrosion resistant?

  1. A zinc coating
  2. A thin, self-healing chromium oxide passive film
  3. Its high carbon content
  4. A paint layer
Show answer & solution

Answer: (B) A thin, self-healing chromium oxide passive film

At least about 10.5% chromium is needed.

Question 3

What is the difference between type 304 and type 316 stainless steel?

  1. 304 contains molybdenum
  2. 304 is not stainless
  3. 316 contains molybdenum, giving better resistance to chloride pitting
  4. 316 has no nickel
Show answer & solution

Answer: (C) 316 contains molybdenum, giving better resistance to chloride pitting

Both are austenitic stainless steels.

Question 4

Why are low-carbon grades such as 304L and 316L used for welded equipment?

  1. They resist sensitisation and intergranular corrosion after welding
  2. They are stronger at high temperature
  3. They are cheaper than carbon steel
  4. They are magnetic
Show answer & solution

Answer: (A) They resist sensitisation and intergranular corrosion after welding

Low carbon limits chromium carbide formation at grain boundaries.

Question 5

What is sensitisation of austenitic stainless steel?

  1. Hardening by cold work
  2. Loss of nickel
  3. Formation of a passive film
  4. Chromium carbide precipitation at grain boundaries when heated in about 425–850 °C, depleting chromium nearby
Show answer & solution

Answer: (D) Chromium carbide precipitation at grain boundaries when heated in about 425–850 °C, depleting chromium nearby

It leads to intergranular corrosion.

Question 6

What is chloride stress corrosion cracking?

  1. Uniform corrosion of carbon steel
  2. Pitting of copper
  3. Erosion of pumps
  4. Cracking of austenitic stainless steels under tensile stress in hot chloride environments
Show answer & solution

Answer: (D) Cracking of austenitic stainless steels under tensile stress in hot chloride environments

Duplex steels and high-nickel alloys resist it better.

Question 7

What is pitting corrosion?

  1. Corrosion between metals
  2. Cracking under stress
  3. Localised attack forming small deep cavities, often caused by chlorides on passive metals
  4. Uniform thinning
Show answer & solution

Answer: (C) Localised attack forming small deep cavities, often caused by chlorides on passive metals

It is dangerous because little metal loss can cause leaks.

Question 8

What is crevice corrosion?

  1. Corrosion due to flow
  2. Localised corrosion in narrow gaps such as under gaskets or deposits
  3. Uniform corrosion
  4. Corrosion at high temperature only
Show answer & solution

Answer: (B) Localised corrosion in narrow gaps such as under gaskets or deposits

Oxygen depletion in the crevice drives it.

Question 9

What is galvanic corrosion?

  1. Accelerated corrosion of the less noble metal when two dissimilar metals are in electrical contact in an electrolyte
  2. Corrosion of a single metal uniformly
  3. Corrosion caused by bacteria only
  4. Corrosion at high temperature
Show answer & solution

Answer: (A) Accelerated corrosion of the less noble metal when two dissimilar metals are in electrical contact in an electrolyte

A large cathode and small anode area is most severe.

Question 10

Which metal corrodes when zinc and steel are coupled in seawater?

  1. Steel
  2. Both equally
  3. Neither
  4. Zinc
Show answer & solution

Answer: (D) Zinc

Zinc is anodic to steel; this is the basis of galvanising.

Question 11

What is cathodic protection?

  1. Using thicker metal
  2. Protecting a metal by making it the cathode, using sacrificial anodes or impressed current
  3. Painting the metal
  4. Adding inhibitors only
Show answer & solution

Answer: (B) Protecting a metal by making it the cathode, using sacrificial anodes or impressed current

It is widely used on buried pipelines and tank bottoms.

Question 12

Which metals are used as sacrificial anodes?

  1. Lead and tin
  2. Copper and silver
  3. Zinc, magnesium and aluminium alloys
  4. Platinum and gold
Show answer & solution

Answer: (C) Zinc, magnesium and aluminium alloys

They are more active than steel.

Question 13

What is erosion–corrosion?

  1. Accelerated attack due to combined fluid velocity and corrosion, removing protective films
  2. Cracking under stress
  3. Corrosion at welds only
  4. Corrosion in stagnant water
Show answer & solution

Answer: (A) Accelerated attack due to combined fluid velocity and corrosion, removing protective films

It occurs at elbows, pump impellers and valve trims.

Question 14

What is hydrogen embrittlement?

  1. Coating with hydrogen
  2. Corrosion by hydrogen gas at low temperature only
  3. Loss of ductility of steel caused by absorbed atomic hydrogen
  4. Hardening by heat treatment
Show answer & solution

Answer: (C) Loss of ductility of steel caused by absorbed atomic hydrogen

It can cause sudden cracking of high-strength steels.

Question 15

Which standard specifies materials for resisting sulphide stress cracking in sour (H₂S) oil and gas service?

  1. ASME B31.1
  2. NACE MR0175 / ISO 15156
  3. ISO 9001
  4. API 650
Show answer & solution

Answer: (B) NACE MR0175 / ISO 15156

It limits hardness of steels and welds.

Question 16

What is high-temperature hydrogen attack?

  1. Reaction of hydrogen with carbon in steel at high temperature and pressure, forming methane and fissures
  2. Rusting in water
  3. Caustic cracking
  4. Pitting by chlorides
Show answer & solution

Answer: (A) Reaction of hydrogen with carbon in steel at high temperature and pressure, forming methane and fissures

Nelson curves (API 941) guide steel selection.

Question 17

What is caustic embrittlement?

  1. Corrosion of copper in ammonia
  2. Erosion by slurries
  3. Pitting of stainless steel by chlorides
  4. Stress corrosion cracking of carbon steel in hot concentrated alkaline solutions
Show answer & solution

Answer: (D) Stress corrosion cracking of carbon steel in hot concentrated alkaline solutions

It was historically seen in riveted boilers.

Question 18

What is creep?

  1. Fatigue under cyclic load
  2. Slow, time-dependent plastic deformation of a material under stress at high temperature
  3. Corrosion at room temperature
  4. Sudden brittle fracture
Show answer & solution

Answer: (B) Slow, time-dependent plastic deformation of a material under stress at high temperature

Furnace tubes are designed for creep life.

Question 19

What is fatigue failure?

  1. Failure under repeated cyclic stresses below the static strength
  2. Corrosion failure
  3. Failure under constant load at high temperature
  4. Failure due to buckling
Show answer & solution

Answer: (A) Failure under repeated cyclic stresses below the static strength

Vibrating piping often fails by fatigue.

Question 20

What is the ductile-to-brittle transition temperature?

  1. The melting point
  2. The annealing temperature
  3. The creep temperature
  4. The temperature below which a steel loses toughness and may fracture in a brittle manner
Show answer & solution

Answer: (D) The temperature below which a steel loses toughness and may fracture in a brittle manner

Low-temperature service needs fine-grain or nickel steels.

Question 21

Which material is commonly used for handling concentrated sulphuric acid (above about 93%) at ambient temperature?

  1. Aluminium
  2. Copper
  3. Carbon steel
  4. Zinc
Show answer & solution

Answer: (C) Carbon steel

A protective iron sulphate film forms; velocity must be limited.

Question 22

Which material is commonly used for concentrated nitric acid storage?

  1. Copper
  2. Zinc
  3. Carbon steel
  4. Aluminium or stainless steel
Show answer & solution

Answer: (D) Aluminium or stainless steel

Carbon steel is rapidly attacked by dilute nitric acid.

Question 23

Which metal is preferred for hot concentrated caustic soda service?

  1. Nickel or high-nickel alloys
  2. Copper
  3. Aluminium
  4. Zinc
Show answer & solution

Answer: (A) Nickel or high-nickel alloys

Aluminium is rapidly attacked by alkalis.

Question 24

Which alloy is widely used for hydrofluoric acid service?

  1. Aluminium
  2. Carbon steel at high velocity
  3. Monel (nickel–copper alloy)
  4. Glass
Show answer & solution

Answer: (C) Monel (nickel–copper alloy)

Glass is attacked by HF.

Question 25

Which metal has excellent resistance to seawater and wet chlorine?

  1. Carbon steel
  2. Titanium
  3. Zinc
  4. Aluminium
Show answer & solution

Answer: (B) Titanium

It is used in condenser tubes and chlorine plants.

Question 26

Why is glass-lined steel used in pharmaceutical reactors?

  1. It resists most acids and is easy to clean while steel gives strength
  2. It conducts heat best
  3. It resists hot strong alkalis well
  4. It resists hydrofluoric acid
Show answer & solution

Answer: (A) It resists most acids and is easy to clean while steel gives strength

It is attacked by HF and hot concentrated alkalis.

Question 27

What is the main limitation of PTFE linings?

  1. High cost of steel
  2. Poor chemical resistance
  3. Limited mechanical strength and temperature of about 200–260 °C
  4. Electrical conductivity
Show answer & solution

Answer: (C) Limited mechanical strength and temperature of about 200–260 °C

PTFE resists almost all chemicals.

Question 28

What is fibre-reinforced plastic (FRP) often used for?

  1. High-pressure steam lines
  2. Cryogenic service
  3. High-temperature furnace tubes
  4. Tanks, ducts and pipes for corrosive chemicals and water at moderate temperatures
Show answer & solution

Answer: (D) Tanks, ducts and pipes for corrosive chemicals and water at moderate temperatures

It is light and corrosion resistant.

Question 29

What is a corrosion inhibitor?

  1. A coating of zinc
  2. A chemical added in small amounts to reduce the corrosion rate of a metal in a fluid
  3. A thicker wall
  4. A cathodic protection anode
Show answer & solution

Answer: (B) A chemical added in small amounts to reduce the corrosion rate of a metal in a fluid

Filming amines are used in refinery overhead systems.

Question 30

What is the usual unit of corrosion rate?

  1. Pascals
  2. Millimetres per year (or mils per year)
  3. Kelvin per minute
  4. Kilograms per hour
Show answer & solution

Answer: (B) Millimetres per year (or mils per year)

Less than 0.1 mm/year is usually considered good resistance.

Question 31

What is the corrosion allowance for 20 years of service if corrosion rate is 0.1 mm per year?

  1. 0.1 mm
  2. 0.5 mm
  3. 2 mm
  4. 20 mm
Show answer & solution

Answer: (C) 2 mm

Allowance = rate × design life.

Question 32

What does a Pourbaix diagram show?

  1. Temperature against time
  2. Corrosion rate against time
  3. Stress against strain
  4. Regions of immunity, corrosion and passivity of a metal as functions of potential and pH
Show answer & solution

Answer: (D) Regions of immunity, corrosion and passivity of a metal as functions of potential and pH

It is a thermodynamic guide, not a rate predictor.

Question 33

Which alloy family is used for high-temperature furnace tubes in steam reformers?

  1. Centrifugally cast high-nickel–chromium alloys such as HP-modified
  2. Brass
  3. Carbon steel
  4. Aluminium
Show answer & solution

Answer: (A) Centrifugally cast high-nickel–chromium alloys such as HP-modified

They resist creep and oxidation near 900–1,000 °C.

Question 34

What is duplex stainless steel?

  1. A copper alloy
  2. Carbon steel with chromium plating
  3. Stainless steel with a mixed austenitic and ferritic structure, offering high strength and chloride resistance
  4. Steel coated twice
Show answer & solution

Answer: (C) Stainless steel with a mixed austenitic and ferritic structure, offering high strength and chloride resistance

It is used in offshore and seawater systems.

Question 35

What is microbiologically influenced corrosion (MIC)?

  1. Corrosion accelerated by bacteria such as sulphate-reducing bacteria
  2. Corrosion by acids only
  3. Corrosion due to microscopes
  4. Corrosion at high temperature
Show answer & solution

Answer: (A) Corrosion accelerated by bacteria such as sulphate-reducing bacteria

It is common in stagnant water systems and pipelines.

Question 36

What is the typical maximum service temperature of carbon steel for pressure parts before creep becomes significant?

  1. About 100 °C
  2. About 425 °C
  3. About 900 °C
  4. About 1,200 °C
Show answer & solution

Answer: (B) About 425 °C

Alloy steels such as Cr–Mo are used above this.

Question 37

Which alloy steels are used for high-temperature hydrogen service and steam lines?

  1. Zinc
  2. Copper
  3. Chromium–molybdenum steels such as 1¼Cr–½Mo and 2¼Cr–1Mo
  4. Plain aluminium
Show answer & solution

Answer: (C) Chromium–molybdenum steels such as 1¼Cr–½Mo and 2¼Cr–1Mo

They resist creep and hydrogen attack.

Question 38

Which materials are used for cryogenic service such as LNG at −162 °C?

  1. Cast iron
  2. Ordinary concrete only
  3. Plain carbon steel
  4. 9% nickel steel, austenitic stainless steel or aluminium alloys
Show answer & solution

Answer: (D) 9% nickel steel, austenitic stainless steel or aluminium alloys

They keep their toughness at very low temperatures.

Question 39

Why is cast iron unsuitable for pressure parts in hazardous service?

  1. It is too ductile
  2. It is too expensive
  3. It corrodes faster than steel always
  4. It is brittle and may fail suddenly
Show answer & solution

Answer: (D) It is brittle and may fail suddenly

It is still used for some low-pressure water pumps.

Question 40

What is the main use of copper alloys such as admiralty brass in heat exchangers?

  1. Concentrated sulphuric acid
  2. Ammonia service
  3. Condenser and cooler tubes for water service
  4. High-temperature furnace tubes
Show answer & solution

Answer: (C) Condenser and cooler tubes for water service

Copper alloys are attacked by ammonia.

Question 41

What is dezincification?

  1. Selective leaching of zinc from brass, leaving porous copper
  2. Galvanising
  3. Corrosion of zinc anodes
  4. Coating with zinc
Show answer & solution

Answer: (A) Selective leaching of zinc from brass, leaving porous copper

Inhibited brasses resist it.

Question 42

What is the principle of corrosion protection by painting?

  1. Making the metal cathodic
  2. Increasing wall thickness
  3. Removing oxygen from water
  4. Creating a barrier between the metal and the corrosive environment
Show answer & solution

Answer: (D) Creating a barrier between the metal and the corrosive environment

Zinc-rich primers add sacrificial protection.

Question 43

Why is hot-dip galvanising applied to structural steel in plants?

  1. The zinc coating provides barrier and sacrificial protection against atmospheric corrosion
  2. It increases conductivity
  3. It increases strength
  4. It makes steel stainless
Show answer & solution

Answer: (A) The zinc coating provides barrier and sacrificial protection against atmospheric corrosion

It is widely used for pipe racks and gratings.

Practice these 43 questions interactively →